Curing takes place at | ||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Temperature | 90 - 180 °C | |||||||||||||
Pressure | 50 - 60 bar | |||||||||||||
Time | 10 - 15 min |
To prevent hot embedding resin from adhering to the punch of the press, brush the press cylinder with Solilub.
Solilub powder prevents the hot embedding material from sticking to the punch of the hot embedding press.